The improvement of the compatibility of natural rubber (NR)/acrilonitrile-butadiene rubber (NBR) blend onrubber seal vulcanizate has been done by the addition of chloroprene rubber (CR) or epoxidized natural rubber(ENR) as compatibilizer. Rubber seal compound was made of NR and NBR blend (BN) with CR (BCR), and ENRwith epoxy content of 10% (BENR10), 20% (BENR20), 30% (BENR30), 40% (BENR40), and 50% (BENR50). Thecomposition in each formula was homogenized, with comparison of NR:NBR at 40:60, and NR:compatibilizer:NBRat 40:5:55. That compounds were vulcanized with efficient system at 150oC. The addition of CR-compatilizerimproved the curing characteristic, compression set, and n-pentane resistance of BN vulcanizate. Meanwhile, theaddition of KAE-compatilizer improved the elasticity of BN vulcanizate. BENR elasticity and n-pentane resistanceincreased in line with the increasing level of epoxy content of ENR.Peningkatan kompatibilitas pencampuran karet alam (KA) dan akrilonitril-butadiena (NBR) pada vulkanisatkaret perapat dilakukan dengan menambahkan kompatibiliser karet kloroprena (CR) atau karet alam epoksidasi(KAE). Kompon karet perapat dibuat dari campuran KA dan NBR (BN) dengan kompatibiliser CR (BCR) danKAE dengan kandungan epoksi 10% (BKAE10), 20% (BKAE20), 30% (BKAE30), 40% (BKAE40), dan 50%(BKAE50). Komposisi pada masing-masing formula diseragamkan dengan perbandingan KA:NBR sebesar 40:60dan KA:kompatibiliser:NBR sebesar 40:5:55. Kompon divulkanisasi dengan sistem efisien pada suhu 1500C.Penambahan kompatibiliser CR memperbaiki karakteristik pematangan, pampatan tetap, dan ketahanan n-pentanavulkanisat KA/NBR (BN). Sedangkan penambahan kompatibiliser KAE memperbaiki sifat elastis vulkanisat.Keelastisan dan ketahanan n-pentana BKAE meningkat seiiring kandungan epoksi KAE. |