Deskripsi Lengkap
Bahasa : | ind |
Sumber Pengatalogan : | LibUI ind rda |
Tipe Konten : | text (rdacontent) |
Tipe Media : | unmediated (rdamedia); computer (rdamedia) |
Tipe Carrier : | volume (rdacarrier); online resource (rdacarrier) |
Deskripsi Fisik : | xv, 41 pages : illustration ; 28 cm + appendix |
Naskah Ringkas : | |
Lembaga Pemilik : | Universitas Indonesia |
Lokasi : | Perpustakaan UI, Lantai 3 |
- Ketersediaan
- File Digital: 1
- Ulasan
- Sampul
- Abstrak
No. Panggil | No. Barkod | Ketersediaan |
---|---|---|
S67197 | 14-19-052774010 | TERSEDIA |
Tidak ada ulasan pada koleksi ini: 20457227 |
Abstrak
Perkembangan teknologi serta penggunaannya yang pesat membuat meningkatnya jumlah limbah elektronik global, salah satunya adalah limbah printed circuit board PCB . Limbah PCB dipersiapkan dengan mengominusi hingga ukuran partikel 1-2 cm2. Limbah yang telah dikominusi dilindi dengan menggunakan campuran asam klorida 0,5 M dan hidrogen peroksida 0,4 M sebagai pelarut dan hasilnya diuji Atomic Absorption Spectrophotometer AAS.
Hasil analisis pelindian menunjukan peningkatan kadar emas mencapai 33,24 dan tembaga mencapai 24,60 . Hasil pelindian diadsorpsi dengan karbon aktif dengan variasi konsentrasi 10, 20, 25, 30, dan 50 g/L. Hasil adsorpsi dianalisis dengan AAS dan menunjukan peningkatan kadar emas mencapai 99,1 pada konsentrasi karbon aktif 50 g/L.
Advancement in technology and the increasing of its demand increase the amount of electronic waste especially printed circuit board PCB . Waste PCB was comminuted to particle size of 1 2 cm2. Comminuted waste PCB was leached in the mixture of 0,5 M hydrochloric acid and 0,4 M hydrogen peroxide as lixiviants and the result was tested using Atomic Absorption Spectrophotometer AAS. The result showed that the gold recovery is 33.24 and copper 24.60 . Adsorption was done using activated carbon with the concentration of 10, 20, 25, 30, and 50 g L. The filtrate then was tested using AAS and showed that 99.1 of gold was recovered in the adsorption using 50 g L activated carbon.
Advancement in technology and the increasing of its demand increase the amount of electronic waste especially printed circuit board PCB . Waste PCB was comminuted to particle size of 1 2 cm2. Comminuted waste PCB was leached in the mixture of 0,5 M hydrochloric acid and 0,4 M hydrogen peroxide as lixiviants and the result was tested using Atomic Absorption Spectrophotometer AAS. The result showed that the gold recovery is 33.24 and copper 24.60 . Adsorption was done using activated carbon with the concentration of 10, 20, 25, 30, and 50 g L. The filtrate then was tested using AAS and showed that 99.1 of gold was recovered in the adsorption using 50 g L activated carbon.