 Abstrak

ABSTRACT
Krisis energi dunia dan tingginya harga sumber energi fosil di Eropa dan negara barat menyebabkan innovasi dalam pemanfaatan energi alternatif yang tidak menimbulkan polusi udara CO2 maupun radio aktif. Sehingga diperlukan sumber energi baru, salah satunya adalah solar sel. CdS merupakan salah satu komponen penting sel surya lapis tipis. Pada pembuatan CdS sebagai lapisan buffer sel surya lapis tipis berbasis CZTS dilakukan dengan metode chemical bath deposition (CBD). CdS dideposisikan pada kaca terlapis CZTS dengan variable yang berbeda untuk mendapatkan kondisi deposisi yang optimal. Deposisi CdS telah berhasil dilakukan, dan temperatur optimalnya adalah 90°C. Temperatur dibawah 90°C akan menghasilkan lapisan antar muka yang dapat mengurangi sifat transmitansi lapisan CdS. Konsentrasi optimal pada [S]:[Cd] = 5, karena memiliki nilai transmitansi terbaik.

ABSTRACT
The world energy crisis and the high price of fossil energy sources in Europe and the western countries have led to innovation in the use of alternative energy that does not cause CO2 or radioactive air pollution. So that new energy sources are needed, one of which is solar cells. CdS is one of the important components of thin film solar cells. In making CdS as CZTS thin layer solar cell buffer layer was carried out by chemical bath deposition (CBD) method. CdS is positioned on CZTS coated glass with different variables to obtain optimal deposition conditions. CdS deposition has been successfully carried out, and the optimal temperature is 90°C. Temperatures below 90°C will produce an interface layer that can reduce the transmittance properties of the CdS layer. The optimal concentration at [S]: [Cd]=5, because it has the best transmittance value.

 File Digital: 1

Shelf
 S-pdf-Aldo Perwira Agung.pdf :: Unduh

LOGIN required

 Metadata

No. Panggil : S-Pdf
Entri utama-Nama orang :
Entri tambahan-Nama orang :
Entri tambahan-Nama badan :
Subjek :
Penerbitan : [Place of publication not identified]: [Publisher not identified], 2019
Program Studi :
Bahasa : ind
Sumber Pengatalogan : LibUI ind rda
Tipe Konten : text
Tipe Media : computer
Tipe Carrier : online resource
Deskripsi Fisik : xii, 37 pages : illustration ; appendix
Naskah Ringkas :
Lembaga Pemilik : Universitas Indonesia
Lokasi : Perpustakaan UI, Lantai 3
  • Ketersediaan
  • Ulasan
No. Panggil No. Barkod Ketersediaan
S-Pdf 14-20-601748389 TERSEDIA
Ulasan:
Tidak ada ulasan pada koleksi ini: 20482606