Oktafinaldo Syafza
Studi pemudaran komposisi 0,120 Wt. % Ti dan 0,018 Wt. % Sr terhadap karakteristik paduan AC4B hasil low pressure die casting = Study of fading of AC4B alloy containing 0.120 wt. % Ti and 0.018 wt. % Sr produced by low pressure die casting
Fakultas Teknik Universitas Indonesia, 2009
 UI - Skripsi (Open)
Nike Lestari
Studi pengaruh kombinasi komposisi 0,1 Wt. % Ti dan 0,003, 0,018 dan 0,025 Wt. % Sr terhadap karakteristik paduan AC4B hasil low pressure die casting = Study on combination effect 0.1 wt. % Ti and 0.003, 0.018 and 0.025 wt. % Sr on characteristic of AC4B alloy produced by low pressure die casting
Fakultas Teknik Universitas Indonesia, 2009
 UI - Skripsi (Open)
Febrian Hendra Kurniawan
Pengaruh penambahan 0.067, 0.081, dan 0.115 wt. % Ti terhadap karakteristik paduan AC4B hasil low pressure die casting (LPDC) = Effect of addition 0.067, 0.081 and 0.115 wt. % Ti on characteristic of AC4B alloy produced by low pressure die casting
Fakultas Teknik Universitas Indonesia, 2008
 UI - Skripsi (Open)
Mashudi Darta
Studi pengaruh kombinasi komposisi 0,02 wt% Sr dan 0,055, 0,078 dan 0,087 wt% Ti terhadap ketahanan aus paduan aluminium AC4B = Effect of composition combination of 0.02 wt.% Sr and 0.055, 0.078, and 0.087 wt.% Ti to wear resistance of aluminum alloy AC4B
Fakultas Teknik Universitas Indonesia, 2010
 UI - Skripsi (Open)
M. Husni Harion
Studi pengaruh penambahan 0.019 wt % TI dan 0.029 wt % TI terhadap karakteristik material paduan aluminium AC4B dengan proses low pressure die casting = Study on effect of addition 0.019 wt % TI and 0.029 wt % TI to characteristic of material aluminium alloy AC4B with low pressure die casting process
2008