Oktafinaldo Syafza
Studi pemudaran komposisi 0,120 Wt. % Ti dan 0,018 Wt. % Sr terhadap karakteristik paduan AC4B hasil low pressure die casting = Study of fading of AC4B alloy containing 0.120 wt. % Ti and 0.018 wt. % Sr produced by low pressure die casting
Fakultas Teknik Universitas Indonesia, 2009
 UI - Skripsi Open
Mohammad Azi Fallah
Studi pengaruh kombinasi komposisi 0,02 wt. % Sr dan 0,063, 0,083 dan 0,108 wt. % Ti terhadap karakteristik paduan aluminium AC4B hasil proses low pressure die casting ( LPDC) = Effect of combination of composition of 0.02 wt. % Sr and 0.063, 0.083 and 0.108 wt. % Ti in aluminium AC4B alloy produced by low pressure die casting (LPDC)
Fakultas Teknik Universitas Indonesia, 2009
 UI - Skripsi Open
Febrian Hendra Kurniawan
Pengaruh penambahan 0.067, 0.081, dan 0.115 wt. % Ti terhadap karakteristik paduan AC4B hasil low pressure die casting (LPDC) = Effect of addition 0.067, 0.081 and 0.115 wt. % Ti on characteristic of AC4B alloy produced by low pressure die casting
Fakultas Teknik Universitas Indonesia, 2008
 UI - Skripsi Open
Daniel Julian Kharistal
Studi pengaruh penambahan penghalus butir titanium dengan kadar 0.0505 wt. % dan 0.072 wt. % terhadap karakteristik paduan AC4B hasil low pressure die casting = Study on effects of 0.0505 wt. % and 0.072 wt. % titanium grain refiner on characteristics of AC4B alloy produced by low pressure die casting
Fakultas Teknik Universitas Indonesia, 2008
 UI - Skripsi Open
M. Husni Harion
Studi pengaruh penambahan 0.019 wt % TI dan 0.029 wt % TI terhadap karakteristik material paduan aluminium AC4B dengan proses low pressure die casting = Study on effect of addition 0.019 wt % TI and 0.029 wt % TI to characteristic of material aluminium alloy AC4B with low pressure die casting process
2008